Process Gas Line Elbow Repair

OBJECTIVE

Repair internal wall loss due to Internal corrosion on the extrados of an elbow of a process gas line.

DESIGN DATA

  • Pressure 130 Bar
  • Temperature -10 to 90 °C
  • 3 years design life
  • Fuze-Dry™ Glass Fibre
  • ST3 mechanical surface preparation

EXECUTION

  • Crew of 1x FUZE Field Supervisor
  • Immediate mobilisation

Outcome

  • The engineered repair was completed on time and met ISO 24817

Share: